Vac Aero Awarded Contract for Pressure Quench Vacuum Furnace

INDUSTRIAL HEATING MAGAZINE, September 27, 2004

Vac Aero International Inc. (Oakville, Ontario, Canada) was awarded a contract to supply a 10-bar pressure quench vacuum furnace to Shin Poong Precision Specialty Steel in Korea. The furnace, which incorporates Vac Aero’s latest advances in hot zone design for high-pressure quenching, will be used for tool and die hardening and brazing applications. As part of the contract, Vac Aero also is supplying installation supervision services through its Korean associate, AeroTech.