Vac Aero Receives Vacuum Furnace Order from Liburdi

INDUSTRIAL HEATING MAGAZINE, April 4, 2002

VAC AERO International Inc., Oakville, Ontario, Canada, received an order for a vacuum furnace from Liburdi Turbine Services LLC for a VAV 5450 HV-2 bottom-loading vacuum furnace for their facility in Davidson, N.C. The furnace has a graphite felt lined work zone of 54 in. diameter and 50 in. high, molybdenum elements, Stokes and Varian vacuum pumps, Honeywell and Allen Bradley controls, a recirculating water system and an IG gas storage tank. The furnace will be installed and commissioned by VAC AERO technicians.