Plasma Spray:

 

Boeing Commercial Aircraft Group:

BMS 10-67, Type I

Pratt & Whitney Canada:

CPW 33-5 on Steel, Nickel and Cobalt Alloys
CPW 33-13 on Steel, Nickel, Cobalt and Titanium Alloys
CPW 33-16 on Steel, Nickel, Cobalt and Titanium Alloys
CPW 33-18 on Steel, Nickel and Cobalt Alloys
CPW 33-35 on Aluminum and Magnesium Alloys
CPW 33-37 on Steel, Nickel, Cobalt, Aluminum and Magnesium Alloys
CPW 33-48 on Steel, Nickel and Cobalt Alloys
CPW 33-48 on Ti and Ti Alloys
CPW 33-78 on Steel, Nickel and Cobalt Alloys
CPW 385 on Steel, Nickel and Cobalt Alloys
CPW 518 on Steel, Nickel, Cobalt Alloys and Titanium Alloys
CPW 672

Siemens Westinghouse

Spec 83263X3: MCrAlY – BN – Polyester Abaradable
Spec 83262A3: CoNiCrAlY
Spec 83342NU: Ceramically Bonded Al Coating with Chromate / Phosphate Top Coat
Spec 83260X1: 410 Stainless Steel
Spec 83262Y4: Stellite 6
Spec 83324Z1: CuNiIn
Spec 83269A4: Chromium Carbide

Inorganic Paint Treatment:

 

Pratt & Whitney Canada:

CPW 420-12, -14, -22, -24, -52, -1A and -2A

Shot Peening:

 

Pratt & Whitney Canada:

AMS 2430 (Steel Shot)
AMS 2430 (Glass Beads)



 