Resources: Education & Training

Vacuum heat treating and Brazing Vacuum heat treating and Brazing Paint Thermal Spray Coatings Resources: Knowledge Base

VAC AERO News, Education & Training

vacuum-furnacesVAC AERO Opens its Second Facility in Poland

First established in 2003 in Kalisz, Poland VAC AERO has now opened a second facility located in the town of Rzeszow in southeast Poland. VAC AERO’s Polish divisions offer vacuum heat  treating and brazing, vacuum carburizing, air plasma spray (APS) and HVOF protective coatings, as well as corrosion and oxidation resistant paint coatings. This will VAC AERO’s sixth vacuum heat treating, brazing and coating facility worldwide.

Vacuum Technology with "The Heat Treat Doctor"

vacuum furnacesTool Steel Carbides

Tool steel heat treatment is based on a simple premise, that to obtain the optimum performance from any given grade, every step of the heat treating process including stress relief, austenitizing, quenching, cryogenic treatment and multiple tempers must be done exactly correct. Absolute control of both process and equipment variability is one of many reasons why vacuum processing is popular in tool steel heat treatment.

Vacuum Brazing with Dan Kay

vacuum furnaceCenterline Eutectics in Ni-brazing

Joint clearances must be tight for effective Ni-brazing. Nickel-based brazing filler metals (BFM) can leave a hard, non-ductile eutectic phase in the middle of a brazed joint. The hard, non-ductile metallurgical phase-structures that form upon solidification of Ni-brazed joints must be carefully controlled, or else they can, and will, result in cracks inside the joint in stressful mechanical or thermal-cycling service inside the joint.

Metallography with George Vander Voort

vacuum-furnaceRevealing the Microstructure of Tool Steels

After we have properly prepared our tool steel specimens, it is generally best to examine them as-polished before etching unless we are simply doing a routine test, for depth of decarburization, degree of spheroidization, and so forth. Examination of selectively etched tool steel microstructures by light microscopy provides more information than standard etchants, such as nital, picral or Vilella’s reagent.

The Monty, August 2003 Issue

Sounds like this Johnson & Johnson Company located in Warsaw, Indiana has just purchased a new Vac Aero vacuum furnace. We gather that this unit with a work zone of 16" wide X 12" high and 24" deep and six layers of molybdenum will be used for sintering Titanium bone implants and will mean that when installed Depuy will have a grand total of 12 Vac Aero furnaces worldwide. We also understand that Vac Aero will be doing the complete installation. Combine this order with the Dorssers order mentioned below and it sounds like it was a week for buying vacuum furnaces.

brands
Site design by:
MainlySunny.com
Site powered by: Joomla