The hot zone is perhaps the most critical feature of a vacuum furnace in terms of its affect on furnace performance and operating cost. There are a variety of hot zone designs and the choice of a design should be based on a careful analysis of specific processing applications.
To read the entire article online please visit the Industrial Heating website.
|
|
|
VAC AERO Press Release
AerMet® 100, produced by Carpenter Technology Corporation, is a precipitation hardening alloy based on an iron-cobalt nickel mixture strengthened with carbon, chromium and molybdenum. The alloy is equal in strength to 300M high strength steel but with better fracture toughness and stress corrosion cracking resistance. This makes it ideal for use in aircraft components where weight-savings and reliability in severe environments are critical, such as the landing gear for carrier-based military aircraft.
|
|
|
VAC AERO Press Release
VAC AERO’s Ontario Thermal Processing Division continues to support aircraft landing gear programs large and small.
VAC AERO’s heat treating operation in Oakville, Ontario continues to maintain its position as a world leader in the processing of aircraft landing gear components. VAC AERO is now heat treating critical landing gear components for many large commercial aircraft programs including Boeing 777, 777LR, 747-800 and Airbus A380 (commercial and freighter versions). New contracts for processing Boeing 787 and Airbus A320 landing gear components will be underway this year.
|
|
|
Metal matrix composites are becoming increasingly popular for industrial applications as diverse as aerospace, automotive and electronics. The composites consist of an alloy matrix reinforced with ceramic particles to enhance mechanical properties. Aluminum alloys are especially popular as a matrix material.
|
| |
|
|
All content is copyright © 2007 by VAC AERO International Inc. All rights reserved. |
Company | Terms and Conditions of Use | Privacy Policy | Contact Us
This email was sent to you by VAC AERO International Inc., 1371 Speers Rd., Oakville, ON – L6L 2X5 Canada.
Vac Aero respects your online privacy. If you do not wish to receive future e-mails from us, please click here to unsubscribe or reply to this message with a subject of Unsubscribe and you will be IMMEDIATELY REMOVED.
|
|