* If you are having trouble viewing this e-mail, click here.
* To make sure you continue to receive our e-mails in your inbox (not sent to bulk or junk folders), please add newsletter@vacaeronews.com to your address book. Click here for more information.
* At VAC AERO International Inc., we practice permission-based marketing. To unsubscribe, please click here.
* To log on to the VAC AERO web site, please click here.
July 2008
905-827-4171

VAC AERO Receives its First Vacuum Furnace Order from Bodycote.
vafurnace.gif OAKVILLE, Ontario, (July 17, 2008) – VAC AERO has been awarded an order for two large vacuum furnaces from Bodycote, the world's largest supplier of thermal processing services. The equipment is destined for Bodycote's facility in Berlin, Connecticut. Both vertical, bottom-loading furnaces have work zone areas 72" diameter by 72" high, VAC AERO's unique graphite felt and carbon composite hot zone insulation, and lanthanated molybdenum elements mounted circumferentially and on top and bottom end shields. The furnace operating systems are based on VAC AERO's versatile hybrid control package with SCADA and complete network integration capabilities. VAC AERO has been building heat treating equipment since 1970 and specializes in the design and manufacture of high temperature vacuum furnaces for the global market.

Dayton Process - Fluorocarbon Cleaning Process
vafurnace.gif The Ultimate Cleaning Treatment For Superalloy Repair.

All gas turbine engines require regular overhaul to ensure continued safe operation. During engine overhaul, decisions must be made on whether to replace deteriorated individual parts and assemblies with new components or to repair them. The ultimate decision depends on both technical and commercial criteria. That is, is there a technically sound repair available and, if so, is it economically favorable compared to the cost of a replacement component? Sometimes lack of availability of replacement components may override purely economic criteria.  READ MORE

Loading Practices for Vacuum Processing
vafurnace.gif Once a good fixture design has been developed, careful consideration should next be given to the loading of the workpieces.

Heating in a vacuum depends mostly on the transfer of energy through radiation from the elements to the load. For uniform heating and cooling, it is important that the workpieces are not shielded by one another. Pieces within the load should be evenly spaced to ensure even exposure to radiation. The size, shape and high temperature strength of the workpiece should also be considered during loading. Alloys with complex shapes and relatively low strength at heat treating temperatures may distort during processing. In some cases, it may be necessary to support these components with specially designed fixtures.  READ MORE

 

Company | Terms and Conditions of Use | Privacy Policy | Contact Us
This email was sent to you by VAC AERO International Inc., 1371 Speers Rd., Oakville, ON – L6L 2X5 Canada.
Vac Aero respects your online privacy. If you do not wish to receive future e-mails from us, please click here
to unsubscribe or reply to this message with a subject of Unsubscribe and you will be IMMEDIATELY REMOVED.